DYNAMIC RESPONSE OF WOOD BASED BIO-COMPOSITIES UNDER HIGH ...
At similar mat pressures, when tested at 20 psi, the material formed from 2% CS and 2% MDI at 140 s had the highest yield strength. Samples containing CS had a high average strain rate when compared with other wood samples, and this shows that the CS contributed to the high stain rate of the material.